The Materials(Metal and Alloy) we used in investment casting

GL Metal’s investment casting foundry stands out for its exceptional capability to cater to a diverse array of alloys, adhering to stringent designations and specifications outlined by industry standards such as ASTM, SAE, AISI, ACI, DIN, GOST, EN, ISO, and GB. With a repertoire of over 100 ferrous and non-ferrous alloys, we specialize in casting parts featuring intricate design structures.

Our expertise covers a broad spectrum of materials, including:

  • Gray Cast Iron: HT150 ~ HT350; EN-GJL-100, EN-GJL-150, EN-GJL-200, EN-GJL-250, EN-GJL-300, EN-GJL-350; GG10, GG15, GG20, GG25, GG30, GG40.
  • Ductile Cast Iron (Nodular Iron): GGG40, GGG45, GGG50, GGG60, GGG70, GGG80; EN-GJS-400-18, EN-GJS-400-15, EN-GJS-450-10, EN-GJS-500-7, EN-GJS-600-3, EN-GJS-700-2, EN-GJS-800-2.
  • Carbon Steel: AISI 1020 ~ AISI 1060, WCA, WCB, WCC, C30, C40, C45.
  • Alloy Steel: ZG20SiMn, ZG30SiMn, ZG30CrMo, ZG35CrMo, ZG35SiMn, ZG35CrMnSi, ZG40Mn, ZG40Cr, ZG42Cr, ZG42CrMo, etc.
  • Stainless Steel: 304, 304L, 316, 316L, 1.4401, 1.4408, 1.4301, 1.4305, 1.4307, 1.4404, 1.4571, and more.
  • Duplex Stainless Steel (DSS) and Precipitation Hardening (PH) Stainless Steel
  • Brass, Bronze, and other Copper-based Alloys
  • Nickel Based Alloy: Inconel 625, Inconel 713, Inconel 718, etc., Cobalt Based Alloys
  • Corrosion-resistant Steel, Seawater-resistant Steel, High-temperature Steel, High-tensile Steel, Duplex Stainless Steel.

Our commitment extends to accommodating specific requests and adhering to additional alloys in accordance with ASTM, SAE, AISI, GOST, DIN, EN, ISO, and GB standards. At GL Metal, we pride ourselves on delivering precision and quality across an extensive range of metal casting solutions.

2. Stainless Steel

Austenitic Stainless Steel (300 Series Stainless Steel)
AlloyTensile StrengthMaximum Use TempMelting PointResistance
301515 MPa
(75 Ksi)
871 °C
(1600 °F)
1399-1421°C
(2550-2590°F)
Excellent corrosion resistance
302585 MPa
(85 Ksi)
870˚C
(1,679˚F)
1400-1420 °C
(2550-2590 °F)
Excellent corrosion resistance
303690 MPa
( 100 Ksi)
760˚C
(1,400˚F)
1400-1420 °C
(2550-2590 °F)
Lower corrosion resistance
304621 MPa
(90 Ksi)
870˚C
(1,679˚F)
1,399 – 1,454˚C
(2,550 – 2,650˚F)
CF8/1.4308/
304L621 MPa
(90 Ksi)
870˚C
(1,679˚F)
1,399 – 1,454˚C
(2,550 – 2,650˚F)
CF3
309620 MPa
(89 Ksi)
1000˚C
(1,832˚F)
1400-1455 °C
(2550-2651 °F)
Excellent corrosion resistance
316579 MPa
(84 ksi)
~800˚C
(1,472˚F)
1,371 – 1,399˚C
(2,500 – 2,550˚F)
CF8M/1.4408
316L579 MPa
(84 ksi)
~800˚C
(1,472˚F)
1,371 – 1,399˚C
(2,500 – 2,550˚F)
CF3M
317585 MPa
( 85 Ksi)
816˚C
(1,500˚F)
1,370 – 1,400˚C
(2,500 – 2,550˚F)
Good chloride resistance
321620 MPa
(90Ksi)
816˚C
(1,500˚F)
1,400 – 1,425˚C
(2,550 – 2,600˚F)
Excellent corrosion resistance
347690 MPa
(101 Ksi)
816˚C
(1,500˚F)
1,400 – 1,425˚C
(2,550 – 2,600˚F)
Excellent corrosion resistance
Ferritic Stainless Steels
AlloyTensile StrengthMaximum Use TempMelting PointResistance
405585 MPa
(85Ksi)
815˚C
(1,499˚F)
1,480 – 1,530˚C
(2,700 – 2,790˚F)
Good acid corrosion resistance
408505 MPa
(73 Ksi)
815˚C
(1,499˚F)
1,400 – 1,455˚C
(2,550 – 2,650˚F)
Resists well against most
oxidizing acids and salt spray
409 448MPa
(65 Ksi)
815˚C
(1,499˚F)
1,425 – 1,510˚C
(2,597 – 2,750 F)
Good corrosion resistance
420 760 – 1702 MPa
(110 – 247 Ksi)
427˚C
(800˚F)
1,455 – 1,510˚C
(2,651 – 2,750 F)
Fairly corrosion resistant
430450 MPa
(65 ksi)
815˚C
(1,499˚F)
1,425 – 1,510˚C
(2,597 – 2750˚F)
Good nitric acid resistance
434540 MPa
(78 ksi)
815˚C
(1,499˚F)
1,426 – 1,510˚C
(2,600 – 2750˚F)
Superior pitting resistance
436459 MPa
(67 Ksi)
815˚C
(1,499˚F)
1,425 – 1,510˚C
(2,600 – 2,750˚F)
Excellent citric and nitric
acid corrosion resistance
442515-550 MPa
(77 – 80Ksi)
925-980˚C
(1,700/1,800˚F)
1,065 – 1,120˚C
(1,950 – 1,120˚F)
Good corrosion resistance
444415 MPa
( 60 Ksi)
950˚C
(1,752˚F)
1,405 – 1,495˚C
(2,561 – 2,723˚F)
Good oxidation resistance
Martensit Stainless Steels
AlloyTensile StrengthMaximum Use TempMelting PointResistance
410500 -1400 MPa
(73 – 203 Ksi)
650˚C
(1,202˚F)
1,482 – 1,532˚C
(2,700 – 2,790˚F)
Good corrosion resistance to
air, water, and some chemicals
410S 444 MPa
(64 Ksi)
705˚C
(1,300˚F)
1,482 – 1,532˚C
(2,700 – 2,790˚F)
Good oxidation resistance
416517 MPa
(75 Ksi)
760˚C
(1,400˚F)
1,480 – 1,530˚C
(2,696 – 2,786˚F)
Poor Chloride resistance. Good
resistance to acids, alkalis & fresh water
4201,586 MPa
(230 ksi)
650˚C
(1,202˚F)
1,454 – 1,510˚C
(2,649 – 2,750˚F)
Resistant to mild acids, alkalis,
and water when hardened
440758 MPa
(110 Ksi)
760˚C
(1,400˚F)
1,483˚C
(  2,700˚F)
Limited corrosion resistance
Duplex (Ferritic-Austenitic) Stainless Steels
AlloyTensile StrengthMaximum Use TempMelting PointResistance
2205620 MPa
(90 Ksi)
300˚C
(572˚F)
1,385 – 1,443˚C
(2,525 – 2,630˚F)
Excellent corrosion resistance
2304>600 MPa
(>87 Ksi)
570˚C
(1058˚F)
900 – 1,150˚C
(1,650 – 2,100˚F)
Resistance to corrosion cracking
2507800 MPa
(116 Ksi)
300˚C
(572˚F)
1,350˚C
(2,460˚F)
Excellent chloride corrosion resistance
Precipitation Hardening (PH) Stainless Steels
AlloyTensile StrengthMaximum Use TempMelting PointResistance
17-41103 MPa
(160 Ksi)
316˚C
(600˚F)
1,404 – 1,440˚C
(2,560 – 2,625˚F)
Excellent corrosion resistance
15-51380 MPa
(200 Ksi)
316˚C
(600˚F)
1,404 – 1,440˚C
(2,560 – 2,625˚F)
Excellent corrosion resistance

3. Carbon Steel

ASTM A216 Cast Carbon Steel
AlloyTensile StrengthMaximum Use TempMelting PointResistance
WCA500 MPa
(73 Ksi)
400˚C
(700˚F)
1410 – 1,460˚C
(2,580 – 2,650˚F)
Excellent corrosion resistance
WCB570 MPa
(83 Ksi)
426˚C
(800˚F)
1410 – 1,460˚C
(2,580 – 2,650˚F)
Excellent corrosion resistance
WCC655 MPa
(95 Ksi)
538˚C
(1000˚F)
1410 – 1,460˚C
(2,580 – 2,650˚F)
Excellent corrosion resistance
SAE-AISI 1020 steel 
AlloyTensile StrengthMaximum Use TempMelting PointResistance
1020460 MPa
(63 Ksi)
400˚C
(700˚F)
1420 – 1,460˚C
(2,590 – 2,650˚F)
Excellent corrosion resistance
1020430 MPa
(62 Ksi)
400˚C
(700˚F)
1420 – 1,460˚C
(2,590 – 2,650˚F)
Excellent corrosion resistance

4. Success